Hello everyone, I'm new to this forum and l really love the look of composites, especially carbon fiber.  I wanted to buy a carbon fiber Headliner and looked around the internet, found several companies that sell them but just my luck, none make them for my car. (2002 Honda Civic LX), so i did the next best thing.  I made my own (my first project ever).  Here are some pics to show you guys how it came out.

http://i74.photobucket.com/albums/i261/Razuuk004/Carbon%20Fiber/Headlinercarbonfiber.jpg

http://i74.photobucket.com/albums/i261/Razuuk004/Carbon%20Fiber/Decepticon.jpg

Low and behold, I did such a good job that i created more parts for my car


http://i74.photobucket.com/albums/i261/Razuuk004/Carbon%20Fiber/DoorPanel2.jpg

http://i74.photobucket.com/albums/i261/Razuuk004/Carbon%20Fiber/IMG00691-20120407-20242.jpg

http://i74.photobucket.com/albums/i261/Razuuk004/Carbon%20Fiber/MomoCover.jpg

http://i74.photobucket.com/albums/i261/Razuuk004/Carbon%20Fiber/IMG00789-20120706-1852-1.jpg

http://i74.photobucket.com/albums/i261/Razuuk004/Carbon%20Fiber/IMG00794-20120707-1624.jpg

http://i74.photobucket.com/albums/i261/Razuuk004/Carbon%20Fiber/20130519_120416.jpg

http://i74.photobucket.com/albums/i261/Razuuk004/Carbon%20Fiber/20130519_120424.jpg

http://i74.photobucket.com/albums/i261/Razuuk004/Carbon%20Fiber/20130519_120434.jpg



I also did another headliner for a friend of mine....


http://i74.photobucket.com/albums/i261/Razuuk004/Carbon%20Fiber/20130621_184317.jpg

http://i74.photobucket.com/albums/i261/Razuuk004/Carbon%20Fiber/20130622_113314.jpg

http://i74.photobucket.com/albums/i261/Razuuk004/Carbon%20Fiber/20130622_140159.jpg


so anyways these are just a few of my projects as a newby.  Please let me know what you think!!!
Replies
TomDesign
TomDesign
Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)
Group: Forum Members
Posts: 454, Visits: 2.5K
How you finished on parts? sanding polishing resin? epoxy or polyster?
razuuk004
razuuk004
Forum Guru (54 reputation)Forum Guru (54 reputation)Forum Guru (54 reputation)Forum Guru (54 reputation)Forum Guru (54 reputation)Forum Guru (54 reputation)Forum Guru (54 reputation)Forum Guru (54 reputation)Forum Guru (54 reputation)
Group: Forum Members
Posts: 10, Visits: 26
sand and clear coat using Automtive clear coat. Then sand that down and buff polish.  I use Epoxy resin on the parts.