Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Easy Composites Ltd Technical Support
»
Easy Composites Ltd - General Technical Support
»
High Capacity Vacuum Pump
High Capacity Vacuum Pump
Post Reply
Like
6
High Capacity Vacuum Pump
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Mattctodd
Mattctodd
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 2,
Visits: 7
I have a question about the exhaust gasses/fumes when using the high capacity vacuum pump to degas resins.
I operate in an enclosed space and wonder was wondering are they ok to operate in a small space? Can i attach a hose to the pump to vent the fumes outside?
Thanks
Reply
Like
6
Reply
Matt (Staff)
Matt (Staff)
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 680,
Visits: 1.9K
Hi Anthony,
To keep the forum useful and logical for everyone to use please post a new question as a new topic. Although I'm not 100% sure what you're asking about I'm pretty sure it's not anything to do with our High Capacity Vacuum Pump.
I'd be happy to answer any questions you have but please post as a new topic and be as detailed as you can.
Kind regards, Matt
Matt Statham
Easy Composites / Carbon Mods - Technical Sales
Reply
Like
7
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
High Capacity Vacuum Pump
Mattctodd
-
12 Years Ago
Hi Matt, The pumps being oil filled rotary vane do emit a fine oil mist when operated against a...
Paul (Staff)
-
12 Years Ago
Thanks Matt
Mattctodd
-
12 Years Ago
Please, I need to learn the design calculation for applying epoxy with FRP on beams and column, and...
Anthony
-
12 Years Ago
Hi Anthony, To keep the forum useful and logical for everyone to use please post a new question as...
Matt (Staff)
-
12 Years Ago
Post Reply
Like
6
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search