I have a question about the exhaust gasses/fumes when using the high capacity vacuum pump to degas resins.
I operate in an enclosed space and wonder was wondering are they ok to operate in a small space? Can i attach a hose to the pump to vent the fumes outside?

Thanks
Reply
Paul (Staff)
Paul (Staff)
Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)
Group: Administrators
Posts: 134, Visits: 614
Hi Matt,

The pumps being oil filled rotary vane do emit a fine oil mist when operated against a slight leak or briefly while reaching full vacuum, when running against a properly sealed bag or chamber no mist will be produced once full vacuum has been achieved.

The oil mist is not particularly dangerous in the concentrations likely to be produced during most operations in a well ventilated area, however it is often desirable especially in smaller working spaces to vent the mist, you are perfectly right in thinking of connecting a tube to the pump; the black exhaust cap on the top of the pump has a 'chimney' which is specifically designed so that the pump can be connected to a tube to exhaust the mist elsewhere.

Oil mist filters can also be used on the exhaust, however during prolonged operation these tend to saturate and become ineffective.

I hope this information helps, If you have any further questions please ask.

Paul Statham
Easy Composites / Carbon Mods - Technical
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search