Group: Administrators
Posts: 134,
Visits: 614
|
Hi Philip,
A 1M length of the 2mm x 12mm carbon fibre strip weighs 37grams, the density of the pultrusions is approximatly 1.6, This would mean that in theory it's weight would be 38.4grams however due to the fact that the edges of the pultrusion have a radius, the actual figure is slightly lower.
Paul Statham Easy Composites / Carbon Mods - Technical
|