Technical Support (2.2K reputation)Technical Support (2.2K reputation)Technical Support (2.2K reputation)Technical Support (2.2K reputation)Technical Support (2.2K reputation)Technical Support (2.2K reputation)Technical Support (2.2K reputation)Technical Support (2.2K reputation)Technical Support (2.2K reputation)
Group: Administrators
Posts: 134, Visits: 614
Hi Dogzilla,

Your dead right it's not that hard to weigh the sections and list them so as soon as we have the chance we will do just that, in the mean time your section weighs 8grams in theory and reality.

Paul Statham
Easy Composites / Carbon Mods - Technical
philiplardner
philiplardner
Supreme Being (656 reputation)Supreme Being (656 reputation)Supreme Being (656 reputation)Supreme Being (656 reputation)Supreme Being (656 reputation)Supreme Being (656 reputation)Supreme Being (656 reputation)Supreme Being (656 reputation)Supreme Being (656 reputation)
Group: Awaiting Activation
Posts: 25, Visits: 65
Thanks Paul - exactly what I was looking for.

Paul (Staff) (15/03/2012)
Hi Philip,

A 1M length of the 2mm x 12mm carbon fibre strip weighs 37grams, the density of the pultrusions is approximatly 1.6, This would mean that in theory it's weight would be 38.4grams however due to the fact that the edges of the pultrusion have a radius, the actual figure is slightly lower. 

dogzilla
dogzilla
Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)
Group: Forum Members
Posts: 2, Visits: 7
Is it that hard to weigh each of your products on the site?

At the very least I need to know how much each of the flat strip carbon weighs per meter and I don't see any of that on your site? And I'd rather see the actual recorded weight than the manufacturer "spec".

Whilst I'm here how much does this weight : Carbon Fibre Strip 0.5mm x 10mm 1m (39") [OS1]
Edited 14 Years Ago by dogzilla
Paul (Staff)
Paul (Staff)
Technical Support (2.2K reputation)Technical Support (2.2K reputation)Technical Support (2.2K reputation)Technical Support (2.2K reputation)Technical Support (2.2K reputation)Technical Support (2.2K reputation)Technical Support (2.2K reputation)Technical Support (2.2K reputation)Technical Support (2.2K reputation)
Group: Administrators
Posts: 134, Visits: 614
Hi Philip,

A 1M length of the 2mm x 12mm carbon fibre strip weighs 37grams, the density of the pultrusions is approximatly 1.6, This would mean that in theory it's weight would be 38.4grams however due to the fact that the edges of the pultrusion have a radius, the actual figure is slightly lower. 

Paul Statham
Easy Composites / Carbon Mods - Technical
philiplardner
philiplardner
Supreme Being (656 reputation)Supreme Being (656 reputation)Supreme Being (656 reputation)Supreme Being (656 reputation)Supreme Being (656 reputation)Supreme Being (656 reputation)Supreme Being (656 reputation)Supreme Being (656 reputation)Supreme Being (656 reputation)
Group: Awaiting Activation
Posts: 25, Visits: 65
I would also be interested in seeing the technical data on the 2mm x 12mm pultruded flat bar when you get it.

In the meantime, could you tell me the exact weight (nearest 0.1g if possible) of a 1m length of 2mm x 12mm and 1mm x 6mm pultruded flat bars?

Thanks,

Phil.
Edited 14 Years Ago by philiplardner
Tenson
Tenson
Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)
Group: Forum Members
Posts: 2, Visits: 12
Thanks for your reply. I'll keep an eye on the product pages.

Good work!
Joe
Joe
Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)
Group: Forum Members
Posts: 310, Visits: 1.5K
Matt (Staff) (17/02/2012)

Hi Tenson,

The manufacturer of the pultrusions has been unable to provide us with the mechanicaldata for some time. They're first-rate pulltrusions but for some reason they'rebeen slow getting the mechanical properties over to us. For this reason we'vecommissioned one of the universities that we work with to do their own empiricaltesting and so we should soon have this data. I'll add it to the product pagesas soon as it comes through.

Best regards, Matt



Now thats some serious sellers. DIY'ers now also can have access to some "industry-only" datas. Thanks EC.

 



 


    A $1000 electronic device will always protect a 10 cents fuse
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K

Hi Tenson,

The manufacturer of the pultrusions has been unable to provide us with the mechanical data for some time. They're first-rate pulltrusions but for some reason they've been slow getting the mechanical properties over to us. For this reason we've commissioned one of the universities that we work with to do their own empirical testing and so we should soon have this data. I'll add it to the product pagesas soon as it comes through.

Best regards, Matt



Matt Statham
Easy Composites / Carbon Mods - Technical Sales
Edited 14 Years Ago by Matt (Staff)
Tenson
Tenson
Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)
Group: Forum Members
Posts: 2, Visits: 12
Can you please provide technical data on the pulltruded carbon fibre? I'm looking at the 2mm x 12mm strip.


Specifically I need to know Young's Modulus, Density and Rockwell hardness.

Thank you,
Simon
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search