Can you please provide technical data on the pulltruded carbon fibre? I'm looking at the 2mm x 12mm strip.


Specifically I need to know Young's Modulus, Density and Rockwell hardness.

Thank you,
Simon
Replies
philiplardner
philiplardner
Supreme Being (360 reputation)Supreme Being (360 reputation)Supreme Being (360 reputation)Supreme Being (360 reputation)Supreme Being (360 reputation)Supreme Being (360 reputation)Supreme Being (360 reputation)Supreme Being (360 reputation)Supreme Being (360 reputation)
Group: Awaiting Activation
Posts: 25, Visits: 65
I would also be interested in seeing the technical data on the 2mm x 12mm pultruded flat bar when you get it.

In the meantime, could you tell me the exact weight (nearest 0.1g if possible) of a 1m length of 2mm x 12mm and 1mm x 6mm pultruded flat bars?

Thanks,

Phil.
Edited 13 Years Ago by philiplardner
Paul (Staff)
Paul (Staff)
Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)
Group: Administrators
Posts: 134, Visits: 614
Hi Philip,

A 1M length of the 2mm x 12mm carbon fibre strip weighs 37grams, the density of the pultrusions is approximatly 1.6, This would mean that in theory it's weight would be 38.4grams however due to the fact that the edges of the pultrusion have a radius, the actual figure is slightly lower. 

Paul Statham
Easy Composites / Carbon Mods - Technical
philiplardner
philiplardner
Supreme Being (360 reputation)Supreme Being (360 reputation)Supreme Being (360 reputation)Supreme Being (360 reputation)Supreme Being (360 reputation)Supreme Being (360 reputation)Supreme Being (360 reputation)Supreme Being (360 reputation)Supreme Being (360 reputation)
Group: Awaiting Activation
Posts: 25, Visits: 65
Thanks Paul - exactly what I was looking for.

Paul (Staff) (15/03/2012)
Hi Philip,

A 1M length of the 2mm x 12mm carbon fibre strip weighs 37grams, the density of the pultrusions is approximatly 1.6, This would mean that in theory it's weight would be 38.4grams however due to the fact that the edges of the pultrusion have a radius, the actual figure is slightly lower. 

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search