I had a pattern in a mould that I believed was mechanically locked. Since all was lost, I wanted to remove the pattern and do a thorough postmortem. 

To attempt this I made cuts into the flanged portion as pictured below.

http://www.talkcomposites.com/Uploads/Images/b812df10-c5e0-477d-840c-850e.gif


The 2mm wide cuts reduced the rigidity of mould slightly, and to my surprise the pattern could be removed!!!BigGrin


The mould seems to be pretty good, EXCEPT flange damage - the 2mm wide cuts, hacksaw holes, and loss of some gelcoat at hacksaw holes!!Blush

How do you recommend I repair it? It's still extremely rigid and strong, it just has to cope with a vaccuum bag...

Thanks!
Edited 12 Years Ago by LaxFriedrichs
Replies
Joe
Joe
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 310, Visits: 1.5K
Hi, 

I heared about repairing gelcoat (unimold, at least) with "wax additive", as opposed to cling film. 

We can see that in one of the bonnet video the EC staff made. 

Anyone could explain that? Thx. 

 



 


    A $1000 electronic device will always protect a 10 cents fuse
wojtepanik
wojtepanik
Supreme Being (755 reputation)Supreme Being (755 reputation)Supreme Being (755 reputation)Supreme Being (755 reputation)Supreme Being (755 reputation)Supreme Being (755 reputation)Supreme Being (755 reputation)Supreme Being (755 reputation)Supreme Being (755 reputation)
Group: Forum Members
Posts: 102, Visits: 582
Joe (20/10/2013)
Hi, 

I heared about repairing gelcoat (unimold, at least) with "wax additive", as opposed to cling film. 

We can see that in one of the bonnet video the EC staff made. 

Anyone could explain that? Thx. 
When gelcoat cures on the air some chemical reaction makes gelcoat tacky even chen fully cured and was additive makes gelcoat not tacky even if cured on air.
Wojtek from Poland 

~~~Everytime I hear sound of demoulding part I have eargasm~~~
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
LaxFriedrichs - 12 Years Ago
carboncactus - 12 Years Ago
LaxFriedrichs - 12 Years Ago
carboncactus - 12 Years Ago
LaxFriedrichs - 12 Years Ago
carboncactus - 12 Years Ago
LaxFriedrichs - 12 Years Ago
Joe - 12 Years Ago
wojtepanik - 12 Years Ago
Warren (Staff) - 12 Years Ago
Joe - 12 Years Ago
Joe - 12 Years Ago
wozza - 12 Years Ago
FLD - 12 Years Ago
Joe - 12 Years Ago
carboncactus - 12 Years Ago