how to surface finish EPP?


Author
Message
i9300
i9300
Forum Member (49 reputation)Forum Member (49 reputation)Forum Member (49 reputation)Forum Member (49 reputation)Forum Member (49 reputation)Forum Member (49 reputation)Forum Member (49 reputation)Forum Member (49 reputation)Forum Member (49 reputation)
Group: Forum Members
Posts: 3, Visits: 51
Hi

 I have an original OEM part that is made from EPP, and I need to finish it so that I can use it as a master to pull some composite molds from (ie. fiberglass and CF) is it possible to use just epoxy resin to finish the surface of the EPP or will it react with the EPP and melt it?

Thanks
carboncactus
carboncactus
Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)
Group: Forum Members
Posts: 243, Visits: 1K
No reaction between PP and epoxy. Although you might still need to seal it so that it can release, depending on how dense the foam is. Probably best to wrap it with the lightest glass cloth you can get and wet it with epoxy. After it cures, sand it smooth.

http://www.talkcomposites.com/Uploads/Images/db628ad5-e0e7-47b9-873a-3d84.png
i9300
i9300
Forum Member (49 reputation)Forum Member (49 reputation)Forum Member (49 reputation)Forum Member (49 reputation)Forum Member (49 reputation)Forum Member (49 reputation)Forum Member (49 reputation)Forum Member (49 reputation)Forum Member (49 reputation)
Group: Forum Members
Posts: 3, Visits: 51
Thanks carbon cactus,

 I wasn't sure if it was possible to just wet it with epoxy, sand and polish that and make a mold from it without the cloth.
carboncactus
carboncactus
Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)
Group: Forum Members
Posts: 243, Visits: 1K
you could do that too, it would be weaker. It depends on the geometry of the foam, it might be rigid enough.

http://www.talkcomposites.com/Uploads/Images/db628ad5-e0e7-47b9-873a-3d84.png
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search