By i9300 - 7/11/2013 2:16:27 PM
Hi
I have an original OEM part that is made from EPP, and I need to finish it so that I can use it as a master to pull some composite molds from (ie. fiberglass and CF) is it possible to use just epoxy resin to finish the surface of the EPP or will it react with the EPP and melt it?
Thanks
|
By carboncactus - 7/11/2013 5:11:04 PM
you could do that too, it would be weaker. It depends on the geometry of the foam, it might be rigid enough.
|
|