As the title. Can the GC50 be sprayed using HVLP gun? I have a Apollo Pro Spray 1500. Hoping to only have to use a different needle. What would be the best cleaning method If I can use it?

Ben
Reply
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
The gun we supply uses a 6mm nozzle, so if your gun has a 6mm nozzle then it should in theory work.

Cleaning involves acetone before it cures. Hence why the cup gun uses disposable cups to reduce clean up time.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search