As the title. Can the GC50 be sprayed using HVLP gun? I have a Apollo Pro Spray 1500. Hoping to only have to use a different needle. What would be the best cleaning method If I can use it?
Ben
|
By Matt (Staff) - 7/31/2013 5:44:50 PM
Hi Ben,
Sorry we missed your next question. No, we wouldn't really recommend trying to thin down the GC50. GC50 is already designed as a spray-gel and as such it has quite a high styrene content already.
It's far better to get a nozzle that's appropriate for spraying gelcoats rather than thin the gelcoat beyond where it's supposed to be.