Yes. There is also a more easyto use product from MAP Yachting in France (do not know who distributes them in the UK) called "Bouche pores". It is a 1 component PU paste, which is smeared over the pinholes. After half an hour or so, the residue is sanded away using a scotchbrite. After that, ready to paint!
|