Group: Administrators
Posts: 2.5K,
Visits: 8.5K
|
Hi,
We only stock the 6mm nozzle at present as we have found that to be the best nozzle for the range of products we sell.
Obviously the resin you have isnt one of ours so we havent had the problem of needing bigger nozzles before - and hence don't stock them.
However if the demand for different range nozzles is there, and we can provide them at a competitive price then we may well start supplying them in the future.
You may struggle to spray the resin at all without thinning it down as the biggest nozzle the manufacturer seems to supply is 7.1mm which may still be too big. Thinning it down may be the best option although best to look on the product data sheet to see if it can be done.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|