Gelcoat spraying gun nozzle size?


Author
Message
Harri
Harri
Supreme Being (95 reputation)Supreme Being (95 reputation)Supreme Being (95 reputation)Supreme Being (95 reputation)Supreme Being (95 reputation)Supreme Being (95 reputation)Supreme Being (95 reputation)Supreme Being (95 reputation)Supreme Being (95 reputation)
Group: Forum Members
Posts: 5, Visits: 11
Hi, just bought your gelcoat spraying gun. Im planning on using it with Axson GC1 050 + GC10 epoxy gelcoat which has rather high viscosity. The standard nozzle size didn't work at all. What size would you recommend me? How big can I drill the standard nozzle?
Reply
Harri
Harri
Supreme Being (95 reputation)Supreme Being (95 reputation)Supreme Being (95 reputation)Supreme Being (95 reputation)Supreme Being (95 reputation)Supreme Being (95 reputation)Supreme Being (95 reputation)Supreme Being (95 reputation)Supreme Being (95 reputation)
Group: Forum Members
Posts: 5, Visits: 11
Great, thanks. Do you sell the nozzles as well? I didn't find them at your webshop.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Harri - 12 Years Ago
carboncactus - 12 Years Ago
Harri - 12 Years Ago
             I don't work here dude lol
carboncactus - 12 Years Ago
Harri - 12 Years Ago
Warren (Staff) - 12 Years Ago
fgayford - 12 Years Ago
Harri - 12 Years Ago
carboncactus - 12 Years Ago
Harri - 12 Years Ago
carboncactus - 12 Years Ago
Warren (Staff) - 12 Years Ago