May I know what kind of resin is suitable for making carbon fiber prepreg. i want to make  prepreg by myself, i but not sure what resin can be use and the ratio too.

many thanks,

Liu
Reply
carboncactus
carboncactus
Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)
Group: Forum Members
Posts: 243, Visits: 1K
Prepreg resin systems can be purchased from prepreg manufacturers like PRF composites or amber composites.
They are formulated specially to go off at room temperature anywhere between 1-30 days.
You could of course, just use infusing resin if you're gonna use it straight away.

As for ratios, you should be looking at under 50%, so you need to weigh the carbon. If its a small bit, you might need a jewlers scale.

http://www.talkcomposites.com/Uploads/Images/db628ad5-e0e7-47b9-873a-3d84.png
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search