Post curing times for a large part


Author
Message
stuart321
stuart321
Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)
Group: Forum Members
Posts: 37, Visits: 178
I'll be infusing a pretty substantial sumpguard at the end of the week and interested in any advice on how critical post curing times and temps are for best mechanical strength on a flat panel.

The tech data sheet for IN-2 resin states 24hrs room temp, 60hrs@40, 6hrs@50, 12hrs@60 but for large parts decrease the thermal gradient and increase the post-cure time - I was planning to double the timings IE 2 days room temp 12/12/24hrs for higher temps - does this sound about right?

The stack is 1000 x 900mm  and almost flat, across the whole part will be 2 layers of 300gsm kevlar, 1 layer of CF 200gsm, 1 layer of 3mm soric, 1 layer of CF 450gsm, 1 layer of CF200gsm, additionally in areas which need additional strength or tend to abrade there will be extra soric / CF / kevlar so the stack could be as much as 10 layers thick in a few places.

Any pointers appreciated!
Thanks
Stuart
Replies
stuart321
stuart321
Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)
Group: Forum Members
Posts: 37, Visits: 178
Thanks - I ramped temps pretty gradually and it seems to have come out great.
3.8Kg for the composite parts of the sumpguard and another 900g for ally reinforcers front and back - 5.7Kg vs 11Kg for the previous all ally version!
Will be interesting to see how it stands up to use - abrasion and hard impacts are the two issues although I have added extra layers where it should need it.

Stuart
carbonfibreworks
carbonfibreworks
Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)
Group: Forum Members
Posts: 292, Visits: 4.5K
stuart321 (18/05/2013)
Thanks - I ramped temps pretty gradually and it seems to have come out great.
3.8Kg for the composite parts of the sumpguard and another 900g for ally reinforcers front and back - 5.7Kg vs 11Kg for the previous all ally version!
Will be interesting to see how it stands up to use - abrasion and hard impacts are the two issues although I have added extra layers where it should need it.

Stuart


Stuart that is a serious sump guard, can you name the vehicle it is for ?

Regards Chris

http://www.talkcomposites.com/Uploads/Images/97e08777-693c-4af1-a27a-86cf.png