Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Hand Layup
»
How close should the breather be?
How close should the breather be?
Post Reply
Like
3
How close should the breather be?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
brummelisa
brummelisa
posted 13 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 20,
Visits: 144
I just started vacuum-bagging my CF and I wonder if the breather should only slightly touch the piece or should the breather be all over it?
/ Marcus
Reply
Like
3
Reply
brummelisa
brummelisa
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 20,
Visits: 144
I'm building a bikeframe (to use in triathlon).
I will build each "pole" individually and then join them togeather in a jig.
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
How close should the breather be?
brummelisa
-
13 Years Ago
The piece of breather fabric that you are going to use mast be larger than the part itself. So it...
MJCT
-
13 Years Ago
Thanks. The reason I'm asking is that I don't use a mould and therefor the surface that are facing...
brummelisa
-
13 Years Ago
Please tell as what you are trying to built. It will be easier to advice you. But yeah, if...
MJCT
-
13 Years Ago
I'm building a bikeframe (to use in triathlon). I will build each "pole" individually and then join...
brummelisa
-
13 Years Ago
Ok, you should wrap the breather all around you’re part just like you do with the peal ply....
MJCT
-
13 Years Ago
Ok, so I will cover the whole part then. But won't the breather make it hard to really press the CF...
brummelisa
-
13 Years Ago
Hi, If you wrap your breather all over your part (well, on your peelply, actually), it will give...
Joe
-
13 Years Ago
The reason that I wonder if one should use the breather on the whole part is that I found the guy...
brummelisa
-
13 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search