Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Easy Composites Ltd Technical Support
»
Easy Composites Ltd - Product Specific Pages
»
Carbon Fibre Tube and Section
»
Creating a 3 or 4 section boom using carbon fibre tubing.
Creating a 3 or 4 section boom using carbon fibre tubing.
Post Reply
Like
4
Creating a 3 or 4 section boom using carbon fibre tubing.
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
khalid
khalid
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 1,
Visits: 3
I am looking to create a 4x1.5m (6m total length approx) CF boom around 52mm OD.
Can you create 4 sections that can screw tight into one another to create this long pole?
Reply
Like
4
Reply
Warren (Staff)
Warren (Staff)
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Administrators
Posts: 2.5K,
Visits: 8.5K
Id suggest a 6 inch overlap would be fine to start with but ultimately you would need to experiment and see how it feels.
Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Reply
Like
4
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Creating a 3 or 4 section boom using carbon fibre tubing.
khalid
-
12 Years Ago
We don't stock a tube in the size you mention but do have a couple either side of it. When making...
Warren (Staff)
-
12 Years Ago
Would it be better to use a cut length of 47.5 mm ID or 46mm ID to slide into a length of 50.8 mm ID...
mattv
-
12 Years Ago
47.5mm ID tube has a rough OD of 50.3mm so half a mm difference should be ok. If youre ordering from...
Warren (Staff)
-
12 Years Ago
Hi, I am looking at an application that requires a similar length of pole ,but has to be able to be...
Campbell
-
12 Years Ago
hi, campbelll, we are able to provide customized tubes, please visit our website...
singcomposite
-
11 Years Ago
The overlap size depends on overall length, load, expected directions of stress etc. When bonded...
Warren (Staff)
-
12 Years Ago
The total length needs to 6mtr. It must be able to be broken down to allow for transportation , max...
Campbell
-
12 Years Ago
Id suggest a 6 inch overlap would be fine to start with but ultimately you would need to experiment...
Warren (Staff)
-
12 Years Ago
Hi, I'm looking to construct a camera pole using3 x 2.5m tubes togive me about 6m reach after...
Roy
-
11 Years Ago
Hi, Roy, we are able to provide customized rods and tubes. Please visit us at www.singcomposite.sg
singcomposite
-
11 Years Ago
Hi, khalid , you may take a look at our team, www.singcomposiate.sg. We have extensive experience in...
singcomposite
-
11 Years Ago
Post Reply
Like
4
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search