Creating a 3 or 4 section boom using carbon fibre tubing.


Author
Message
khalid
khalid
Junior Member (9 reputation)Junior Member (9 reputation)Junior Member (9 reputation)Junior Member (9 reputation)Junior Member (9 reputation)Junior Member (9 reputation)Junior Member (9 reputation)Junior Member (9 reputation)Junior Member (9 reputation)
Group: Forum Members
Posts: 1, Visits: 3
I am looking to create a 4x1.5m (6m total length approx) CF boom around 52mm OD.

Can you create 4 sections that can screw tight into one another to create this long pole?

 
Reply
singcomposite
singcomposite
Forum Guru (57 reputation)Forum Guru (57 reputation)Forum Guru (57 reputation)Forum Guru (57 reputation)Forum Guru (57 reputation)Forum Guru (57 reputation)Forum Guru (57 reputation)Forum Guru (57 reputation)Forum Guru (57 reputation)
Group: Forum Members
Posts: 7, Visits: 10
Hi, Roy, we are able to provide customized rods and tubes. Please visit us at www.singcomposite.sg
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
khalid - 12 Years Ago
Warren (Staff) - 12 Years Ago
mattv - 12 Years Ago
Warren (Staff) - 12 Years Ago
Campbell - 12 Years Ago
singcomposite - 11 Years Ago
Warren (Staff) - 12 Years Ago
Campbell - 12 Years Ago
Warren (Staff) - 12 Years Ago
Roy - 11 Years Ago
singcomposite - 11 Years Ago
singcomposite - 11 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search