Hi Warren
Like everything you have to get used to it. I am getting more relaxed using it now. I really like how it sticks to where you put it and the unlimited time you have to work it. I also like how little work it is to prepare the stack. No peelply, no infusion mesh and no resin to mix and infuse.
I tried my 3rd test and seeing I have an autoclave I used it. (yes I know it isn't needed or necessary but I used it anyway)
I used full 29.9 HG vacuum 212 fahrenheit temp 80 PSI pressure maintained for 6 hours.
I was delighted, the part was absolutely perfect and so densely compacted.
I think for my 4th test I am going to follow the advice of a previous poster who said to allow the resin to flow at a reduced temperature 50 c for I think he said 2 hours then at full temp. (no autoclave this time)
Fred
|