hi! guy's can you help me pls. how can i avoid air trap in carbon fiber infusion.
Reply
Like
3
Reply
gelo
gelo
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 3,
Visits: 19
hi! guy's using vacuum infusion. after air drop test for 15 mins. all the necessary air lick was check and is all okay. then i started to infuse the resin for 55mins in the hood there are no air bubbles then check all the lock, after 24hrs demold the hood there are still some air trap under the carbon....
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Air Trap
gelo
-
12 Years Ago
Any more infomation Gelo, is it in the vacuum lines or the part itself? Has the part been...
pk_090
-
12 Years Ago
if hand lay up, you need to use rollers and roll it all thoroughly. buy as many rollers and as many...
brasco
-
12 Years Ago
hi! guy's using vacuum infusion. after air drop test for 15 mins. all the necessary air lick was...
gelo
-
12 Years Ago
Can you post some pictures of the problem areas? It may help us to give better answers/explanations....
wozza
-
12 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search