Unimold coupling coat?


Author
Message
Ail
Ail
Forum Member (33 reputation)Forum Member (33 reputation)Forum Member (33 reputation)Forum Member (33 reputation)Forum Member (33 reputation)Forum Member (33 reputation)Forum Member (33 reputation)Forum Member (33 reputation)Forum Member (33 reputation)
Group: Forum Members
Posts: 5, Visits: 100
Hello all. I live in the states and I'm trying to put together supplies for making a mold using the unimold package as a guide.  I have found a match/similar product from us composites for everything but the coupling coat?  Does anyone know exactly what it is or of any suitable substitutes?  This will be my first attempt so forgive me if this is a stupid question Tongue Thanks for the help!
carboncactus
carboncactus
Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)
Group: Forum Members
Posts: 243, Visits: 1K
Hi Ail,
I was just rummaging through here and seen that nobody answered your question.
If you haven't found out yet, what EC call a "coupling coat" is known in the industry as a skin coat.
In this instance it's just a standard vinyl ester resin (as long as its HDT is adequate)
DSM's Altac 580 is a good choice.
I'm curious as to what your alternatives were.

http://www.talkcomposites.com/Uploads/Images/db628ad5-e0e7-47b9-873a-3d84.png
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search