Group: Forum Members
Posts: 3,
Visits: 8
|
Hi Warren - thanks for your reply. About a year ago I read about a Phenolic resin that was allegedly Ethanol proof. I think it was called Christic 99 but I can't find any record of it now. It's possible I imagined it and it could have just as easily been a vinylester or polyester resin, but from what I remember of the curing process it was most likely Phenolic. If I didn't imagine it, I'm not sure whether whether there is a gel coat that works with Phenolic resins. Possbily a polyester coating would but with reduced fire retardation, which I'd be prepared to live with if it was ethanol proof. Would you have access to any resources to be able to research this further please?
|