Hello all, newbie trying to start a project. Have never done any CF work before but have done my homework.  Sorry in advance for the book, I feel like this could get long winded.  

Ultimate goal: modular retractable spoiler. (Different tops to attach to the base)
Realistic first time goal: replica of stock spoiler

If you are not familiar with the crossfire it has a retractable spoiler that deploys around 100kph this what I would like to recreate in carbon fiber.  My ultimate goal will be to create my own modular spoiler with various different styles.  

This is what the spoiler looks like removed from the car

Top side (about 3ft wide)

Bottom/mount

Mount/bracket close up

Both halves separated top looks to be glass,bottom is metal

My first order of business will be to recreate the stock unit.

My big question here is how to handle the brackets.  This is a spoiler I picked up used so I can tear into it if absolutely needed.  Do I recreate the brackets in carbon and bond everything together? Can I make a mold around them?

That will prob hold me over for now.

Future plans would include how to make some modifications to the base mold (would like to do some diffuser like strips on the bottom instead.

What to use to create an additional lip on the stock spoiler that can be used to make a mold

How to attach the two halves together so the top could  be swapped out with a different style. Etc.

Thanks for any help / guidance you all can provide.  Also I'm located in the US so not sure about the best place for materials.  I love the kits easy composites supplies but not sure how economical shipping and such would be.

Tanks again!
Reply
Ail
Ail
Forum Member (33 reputation)Forum Member (33 reputation)Forum Member (33 reputation)Forum Member (33 reputation)Forum Member (33 reputation)Forum Member (33 reputation)Forum Member (33 reputation)Forum Member (33 reputation)Forum Member (33 reputation)
Group: Forum Members
Posts: 5, Visits: 100
wozza (19/02/2013)
This the Wing I manufacture, it can produce 258 kg of Downforce at 140 mph. The construction is 200grm 2/2 Twill, 190grm Plain Weave, 2mm Soric and 190grm Plain Weave. It is made in two halves (upper/lower) and bonded together. The mounts are eight layers of 200grm bonded together, left hand/right hand.


Wow, that's on a whole other level right there.  Very nice!  Gives me confidence that the carbon should hold up just fine at my measly 80 pounds :p.  I will have to think on how to do the brackets. I've not done any real metal work either (besides hack jobs) so I'm going to have some things to figure out either way.  I suppose the first order of business will be the mould either way.  Will start putting a supply list together. I basically need everything/anything that will need to be used.

Thanks again guys, feeling good about this.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Ail - 12 Years Ago
Philimon - 12 Years Ago
wozza - 12 Years Ago
pk_090 - 12 Years Ago
Ail - 12 Years Ago
Philimon - 12 Years Ago
             I want that lip wing
Rivera - 12 Years Ago
wozza - 12 Years Ago
Ail - 12 Years Ago
wozza - 12 Years Ago
Ail - 12 Years Ago
pk_090 - 12 Years Ago
Rivera - 12 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search