It depends on how clean the resin is.  Any decent quality resin should be ready to go from the can with no filtering needed.

I would be more concerned about dust/debris on the mould surface or in the environment where you are moulding.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
brasco
brasco
Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)
Group: Forum Members
Posts: 192, Visits: 305
is there any advantage to straining the resins before application? like we do for auto paint?
any light colored dust or chunks of resin or dirt could ruin 100's of dollars of materials.

thoughts?

thanks

scott


CarbonFiberCreations



GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search