Group: Forum Members
Posts: 93,
Visits: 651
|
Cheers ,
I have been having a go today joes method hope it turns out ok.
I will have a go with commpressed air next time,
I may have to paint the part now if it comes out the mould dodgey
Ohh well everydays a school day LOL
Thanks for the replies,
PS What can i do to the mould to make it 100% release my carbon part
i have no8 release wax and easylease is there anything better than what i have ???
|