Hey guys let see if you can help me, I am trying to skinned a product, with carbon firbre, I was told to add catalyst to epoxy. Do this really needed? what is the sense of adding catalyst to epoxy if the epoxy is a laminar glue
Reply
dei
dei
Supreme Being (125 reputation)Supreme Being (125 reputation)Supreme Being (125 reputation)Supreme Being (125 reputation)Supreme Being (125 reputation)Supreme Being (125 reputation)Supreme Being (125 reputation)Supreme Being (125 reputation)Supreme Being (125 reputation)
Group: Forum Members
Posts: 15, Visits: 130
Thank a lots everyone, I finally received my carbon firbra it look cute.

I need other help.

My question is what is the best product to coat the polyerster foam before applying epoxy. I want some thing that can grip the polyerster like the car's body work plaster
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
dei - 12 Years Ago
brasco - 12 Years Ago
dei - 12 Years Ago
fgayford - 12 Years Ago
Shaneer22 - 12 Years Ago
Shaneer22 - 12 Years Ago
dei - 12 Years Ago
brasco - 12 Years Ago
brasco - 12 Years Ago
Warren - 12 Years Ago
dei - 12 Years Ago
brasco - 12 Years Ago
Warren (Staff) - 12 Years Ago
wozza - 12 Years Ago
dei - 12 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search