Epoxy, do you need to add catalyst


Author
Message
dei
dei
Supreme Being (125 reputation)Supreme Being (125 reputation)Supreme Being (125 reputation)Supreme Being (125 reputation)Supreme Being (125 reputation)Supreme Being (125 reputation)Supreme Being (125 reputation)Supreme Being (125 reputation)Supreme Being (125 reputation)
Group: Forum Members
Posts: 15, Visits: 130
Hey guys let see if you can help me, I am trying to skinned a product, with carbon firbre, I was told to add catalyst to epoxy. Do this really needed? what is the sense of adding catalyst to epoxy if the epoxy is a laminar glue
Replies
Shaneer22
Shaneer22
Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)
Group: Forum Members
Posts: 156, Visits: 14K
Polyester can be added up to 5%.epoxy are mixed by weight and catalyst,harderner have to be accurate with in the manufactures ratios.
dei
dei
Supreme Being (125 reputation)Supreme Being (125 reputation)Supreme Being (125 reputation)Supreme Being (125 reputation)Supreme Being (125 reputation)Supreme Being (125 reputation)Supreme Being (125 reputation)Supreme Being (125 reputation)Supreme Being (125 reputation)
Group: Forum Members
Posts: 15, Visits: 130
Shaneer22 (16/02/2013)
Polyester can be added up to 5%.epoxy are mixed by weight and catalyst,harderner have to be accurate with in the manufactures ratios.


You are talking about two rasin here right, polyester and epoxy?
what I understood, Polyester dosen't need catalyst hardener and Epoxy does. Do you mean that Epoxy need 5% of hardener by weight?


cheers

Dei
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
dei - 12 Years Ago
brasco - 12 Years Ago
dei - 12 Years Ago
fgayford - 12 Years Ago
Shaneer22 - 12 Years Ago
Shaneer22 - 12 Years Ago
dei - 12 Years Ago
brasco - 12 Years Ago
brasco - 12 Years Ago
Warren - 12 Years Ago
dei - 12 Years Ago
brasco - 12 Years Ago
Warren (Staff) - 12 Years Ago
wozza - 12 Years Ago
dei - 12 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search