Hi

Which epoxy should I buy use for this?

1:
A motorcycle seat-fuel tank monocoque?
It will not be the fuel tank itself, but it will be self-supporting without a subframe,
and thereby it must be able to handle some weight and not flex.
Are "
New Laminating Resin" and/or "original Epoxy Laminating Resin" to be considered
"construction resins" and do they have good enough mechanical properties for this? 

2:
Motorcycle throttle body, hot environment, it will support/house bearings and must have
some chemical resistance.
Very High Temperature Epoxy Resin?

3,
Motorcycle fairings, should be a bit flexible.

THX



http://motoform.blogspot.se

Edited 13 Years Ago by prsw
Replies
Paul (Staff)
Paul (Staff)
Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)
Group: Administrators
Posts: 134, Visits: 614
The Coating resin as we now call it, is perfectly fine for structural parts, it still features really good mechanical properties jst not as high as those of the EL or IN resins.

Paul Statham
Easy Composites / Carbon Mods - Technical
prsw
prsw
Supreme Being (904 reputation)Supreme Being (904 reputation)Supreme Being (904 reputation)Supreme Being (904 reputation)Supreme Being (904 reputation)Supreme Being (904 reputation)Supreme Being (904 reputation)Supreme Being (904 reputation)Supreme Being (904 reputation)
Group: Forum Members
Posts: 112, Visits: 1K
Paul (Staff) (02/02/2012)
The Coating resin as we now call it, is perfectly fine for structural parts, it still features really good mechanical properties jst not as high as those of the EL or IN resins.


ok, EL seems a bit better, but also my question about additive for preferred viscosity?


http://motoform.blogspot.se