Hi
Which epoxy should I buy use for this?
1: A motorcycle seat-fuel tank monocoque? It will not be the fuel tank itself, but it will be self-supporting without a subframe, and thereby it must be able to handle some weight and not flex. Are "New Laminating Resin" and/or "original Epoxy Laminating Resin" to be considered "construction resins" and do they have good enough mechanical properties for this?
2: Motorcycle throttle body, hot environment, it will support/house bearings and must have some chemical resistance. Very High Temperature Epoxy Resin?
3, Motorcycle fairings, should be a bit flexible.
THX
|
By Matt (Staff) - 2/19/2012 5:41:09 PM
Oh, OK, I see. Yes, I guess there are circumstances where a laminating resin would benefit from some thixotropic property (such as laminating upside-down) but they are rare because that gravity defying thixotropic property will be at the expense of fibre wetting. Let me know how you get on.
|
|