wax filleting tools


Author
Message
brasco
brasco
Supreme Being (2.4K reputation)Supreme Being (2.4K reputation)Supreme Being (2.4K reputation)Supreme Being (2.4K reputation)Supreme Being (2.4K reputation)Supreme Being (2.4K reputation)Supreme Being (2.4K reputation)Supreme Being (2.4K reputation)Supreme Being (2.4K reputation)
Group: Forum Members
Posts: 192, Visits: 305
i had no idea such things existed. but they do!
wax filleting tools


CarbonFiberCreations



Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
For many people DIY filleting tools are just as effective. A tile grout smoothing tool or similar is popular as often they have a ball on one end as well as sharper edges for finer work.

For many, the easiest tool is the end of a finger!!! It might not be so precise but for most it is plenty good enough.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
fgayford
fgayford
Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)
Group: Forum Members
Posts: 433, Visits: 1.2K
Hi Brasco
I have seen these tools before. It reminds me to get busy and make my own. I had planned to weld some different sized ball bearings on some stainless rod.
Fred  
ajb100
ajb100
Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)
Group: Forum Members
Posts: 346, Visits: 4.4K
Got mine from east coast fibreglass, they do all 3 for £30 +vat
Matthieu Libeert
Matthieu Libeert
Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
I just use a spoon, have some in differnt sizes and you can choose the right curve you want of the spoon Smile

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




fgayford
fgayford
Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)
Group: Forum Members
Posts: 433, Visits: 1.2K
Matt

Good Idea! Spoons.

I suppose a round nosed butter knife would be useful too. I am going to check the kitchen drawer when my wife is out! Who knows how many fillet tools are in there.

Fred   
brasco
brasco
Supreme Being (2.4K reputation)Supreme Being (2.4K reputation)Supreme Being (2.4K reputation)Supreme Being (2.4K reputation)Supreme Being (2.4K reputation)Supreme Being (2.4K reputation)Supreme Being (2.4K reputation)Supreme Being (2.4K reputation)Supreme Being (2.4K reputation)
Group: Forum Members
Posts: 192, Visits: 305
well it is not that i am lazy or afraid to use my fingers LOL but many years of use, and how many do i have left in them? and nevermind
the cutting hazards of this type of work. just trying to preserve my hands( i ALWAYS take good care of them) and avoid any cuts. CF and sheetmetal
can be like working with machete's sometimes. and thanks for the other ideas as well.

scott


CarbonFiberCreations



GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search