Can silicone rubber be used to make gaskets ?
Can silicone rubber be used to make gaskets ?
Post Reply
Like
3
Can silicone rubber be used to make gaskets ?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Peter at RLI Audio Lab
Peter at RLI Audio Lab
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 2,
Visits: 7
I need to make quite a complex gasget that provides acoustic insulation between two components as well as making up for minor imperfections in connecting the components. The gasket would be a 'fit one' type. Size approximately 200 mm x 50 mm x 3 mm.
Can your silicone rubber be used for this and if so which one is best ?
Reply
Like
3
Warren (Staff)
Warren (Staff)
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Administrators
Posts: 2.5K,
Visits: 8.5K
Either our
CS2 Condensation Cure Silicone Rubber
or our
AdditionCure Silicone Rubber
can both be used to make gaskets and sealing rings.
AdditionCure Silicone Rubber
has a higher temperature resistance, lower shrink and better dimensional accuracy of the two silicones.
Ultimately it depends on the specific application as to wether a condensation cured or addition cured silicone is better for your needs.
Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search