Hello, new here.

Been making some out of autoclave parts in prepreg, but I'm having problems with pinholes. They are very small. Lacquering and sanding time and time again doesn't seem to work. I believe they must be filled. Looking around the web, most products made specifically for the job seem to be American. Does anyone know how to do this efficiently? Needs to be cheap, quick and easy. It will need to be lacquered afterwards for UV protection.

Thanks

http://www.talkcomposites.com/Uploads/Images/db628ad5-e0e7-47b9-873a-3d84.png
Reply
wozza
wozza
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
If you apply any wax based product then you won't be able to clearcoat on top of that. The only way I have been able to get rid of them completely is to keep applying clearcoat and sanding until they are filled level with the surrounding surface. I have also used black shoe polish to fill/conceal the pin holes after clearcoating, not really a fix more of a cheat. But it does tick the cheap and quick boxes.Wink

Warren

Carbon Copies Ltd
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
carboncactus - 12 Years Ago
Jack.Strong - 12 Years Ago
wozza - 12 Years Ago
andygtt - 12 Years Ago
fgayford - 12 Years Ago
brasco - 12 Years Ago
matthieutje65 - 12 Years Ago
brasco - 12 Years Ago
carboncactus - 12 Years Ago
matthieutje65 - 12 Years Ago
carboncactus - 12 Years Ago
matthieutje65 - 12 Years Ago
carboncactus - 12 Years Ago
matthieutje65 - 12 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search