Which is the best to use? As I understand it, if I am painting the parts its ok to use epoxy, but if I plan to leave it unfinished, then its best to use polyester. Is this correct? Also, is it recommended to use a gel coat first then the resin or just go straight resin? I want my parts to be as lite as possible. I am trying to make my parts around .040 - .050 thick. I tried making my first panel just as a test run and it came out ok, but when I go to make my parts for real I want to make sure they are the best they can be. Does anyone have any suggestions or tips?

I attached a pic of what I am trying to replicate. You can see what is carbon here. Bascially all the cosmetic panels and hood are what I want to make.http://www.talkcomposites.com/Uploads/Images/9a1b3922-6a83-40bd-bdbc-b41f.jpg
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
I have no idea why polyester should be better to leave unfinished?
The finish will 99% be the same between epoxy and polyester... the big difference is that epoxy is supposed to be stronger... this is what your looking for I guess Smile
But, polyester is cheaper than epoxy...
I wouldn't use a gelcoat and just go for the epoxy, since your looking for light parts...gelcoat will add some weight.
If you want to paint your parts sand them a bit (or use peelply in your lay-up) then use a plastic primer and add a clearcoat or colorcoat.

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




RRE
RRE
Supreme Being (84 reputation)Supreme Being (84 reputation)Supreme Being (84 reputation)Supreme Being (84 reputation)Supreme Being (84 reputation)Supreme Being (84 reputation)Supreme Being (84 reputation)Supreme Being (84 reputation)Supreme Being (84 reputation)
Group: Forum Members
Posts: 12, Visits: 33
I am being told polyester has better UV protection than epoxy.