Hi,

For my caterham supers even I would like to laminate some windscreen stanchions out of carbon. As these stancions are not flat, they have to be laminated in the correct curve.
Links to the original parts:
http://www.caterhamparts.co.uk/product.php?id_product=1227
http://www.caterhamparts.co.uk/product.php?id_product=1228
 
My intention is to put the parts on the car as they are, without any paint. Therefore my intention is to have both sides flat. The inner side because of laying directly on the aluminum body panel, the outer side because of optical reasons (glossy finish).

May I ask the experienced with which technique I (beginner) should start?

Many thanks in advance Whistling

Regards from cold switzerland,
Markus
Replies
schleeweiss
schleeweiss
Junior Member (24 reputation)Junior Member (24 reputation)Junior Member (24 reputation)Junior Member (24 reputation)Junior Member (24 reputation)Junior Member (24 reputation)Junior Member (24 reputation)Junior Member (24 reputation)Junior Member (24 reputation)
Group: Forum Members
Posts: 4, Visits: 15
is there a possibility to get a flat back without vacuum bagging?
brasco
brasco
Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)
Group: Forum Members
Posts: 192, Visits: 305
CF resin can be painted
to abrade the surface i suggest P400 grit or finer. P1000/P1200 i think would be too fine.


CarbonFiberCreations



GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search