	Group: Administrators 	        
    Posts: 2.5K, 
    Visits: 8.5K 
    
 
          
		     | 
				                       
                 
                
                    
			            Jeffrey raises a good point that where ever you split it, ensure that each mould half is not mechanically locked into place. That curved edge looks to be a good place and if careful, the flash line can be on the corner and easily removed and hidden when cleaning up the part.                 
			            
  				
			            Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant                     
                     
                                            
                         
                    
                  
             |