Group: Forum Members
Posts: 10,
Visits: 320
|
Hi My daughter ask for a specific color for here sewing table. She want a « Tardis » blue. I have the RGB (0,59,111), CMYK (100,55,10,48) or Pantone (2955C) code. I will cast GC3 over a 30mm chipboard using technics described in video « Complete Epoxy Resin Countertop Tutorial ». My questions are how to get this specific color : Did I have to use solid epoxy color pigment or curl pigments ? What is the mix ratio to get this blue ?
|