By macsddau - 11/13/2022 6:29:24 PM
Hi My daughter ask for a specific color for here sewing table. She want a « Tardis » blue. I have the RGB (0,59,111), CMYK (100,55,10,48) or Pantone (2955C) code. I will cast GC3 over a 30mm chipboard using technics described in video « Complete Epoxy Resin Countertop Tutorial ». My questions are how to get this specific color : Did I have to use solid epoxy color pigment or curl pigments ? What is the mix ratio to get this blue ?
|
By macsddau - 12/18/2022 3:15:36 PM
Yesterday, second pour with barriers all around.
 Today, fully cured. Satin finish.
 The sewing is finished.

A good experience.
Some little things to improve the next time: - Use fumed silicat to make a gelcoat for the egdes of the chipboard. - Check the level - Whait more time before removing the barriers. - improvre polishing (need to get a polisher)
|
|