Hello,

Can anyone recommend any alternatives to 2k paints / primers and fillers for sealing bucks etc.  Is seems 1k systems will be problematic with bonding / mould releasing but 2k looks like evil stuff to work with and prohibitive cost wise for me due to the H&S kit required (3 stage filters for breatheable air supplies, secondary compressor, air fed mask etc..).

Is 1k completely off limit or is it just that it's hit-and-miss to avoid problems?
Replies
Philimon
Philimon
Supreme Being (102 reputation)Supreme Being (102 reputation)Supreme Being (102 reputation)Supreme Being (102 reputation)Supreme Being (102 reputation)Supreme Being (102 reputation)Supreme Being (102 reputation)Supreme Being (102 reputation)Supreme Being (102 reputation)
Group: Forum Members
Posts: 14, Visits: 68
jamesw (03/01/2013)
I'm just about to try a 2k epoxy filler/primer in a can from spraymax (you puncture a bladder with a button on the bottom), this one has no dangerous isocyanates and can be sprayed with a standard carbon type mask for working with epoxy,  hopefully that'll polish to a sheen which will be enough to take the mould from, otherwise will then use a gloss coat from them...
Will let you know how I get on over the weekend...

James


Hi James

How did the spraying go? Most curious Smile
jamesw
jamesw
Supreme Being (497 reputation)Supreme Being (497 reputation)Supreme Being (497 reputation)Supreme Being (497 reputation)Supreme Being (497 reputation)Supreme Being (497 reputation)Supreme Being (497 reputation)Supreme Being (497 reputation)Supreme Being (497 reputation)
Group: Forum Members
Posts: 61, Visits: 558

Finally sprayed 3 large patterns with it today - works a treat! nozzle is adjustable for fan size and orientation, sprays a very nice even coat that flashes off quickly, even in 15deg temps, and seems to build well... Have tried wet sanding an area and it produces a nice sheen (I doubt it will polish to a gloss, but i'll give it a go...

Expensive, but an excellent way to avoid conventional 2k (can use a normal epoxy mask) or sending it away

James

Philimon (26/01/2013)
jamesw (03/01/2013)
I'm just about to try a 2k epoxy filler/primer in a can from spraymax (you puncture a bladder with a button on the bottom), this one has no dangerous isocyanates and can be sprayed with a standard carbon type mask for working with epoxy,  hopefully that'll polish to a sheen which will be enough to take the mould from, otherwise will then use a gloss coat from them...
Will let you know how I get on over the weekend...

James


Hi James

How did the spraying go? Most curious Smile

Edited 12 Years Ago by jamesw
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Element6 - 12 Years Ago
jamesw - 12 Years Ago
brasco - 12 Years Ago
neilb - 12 Years Ago
fgayford - 12 Years Ago
brasco - 12 Years Ago
Philimon - 12 Years Ago
jamesw - 12 Years Ago
neilb - 12 Years Ago
jamesw - 12 Years Ago
Philimon - 12 Years Ago
             Pictures? :D
matthieutje65 - 12 Years Ago
jamesw - 12 Years Ago
jamesw - 12 Years Ago
matthieutje65 - 12 Years Ago
Philimon - 12 Years Ago
jamesw - 12 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search