Hello,

Can anyone recommend any alternatives to 2k paints / primers and fillers for sealing bucks etc.  Is seems 1k systems will be problematic with bonding / mould releasing but 2k looks like evil stuff to work with and prohibitive cost wise for me due to the H&S kit required (3 stage filters for breatheable air supplies, secondary compressor, air fed mask etc..).

Is 1k completely off limit or is it just that it's hit-and-miss to avoid problems?
By jamesw - 2/5/2013 9:02:51 PM

Glad it might help! The finish is better than the photo shows Smile

Night and day compared to standard rattle cans - not quite a spray gun mist, but close

Just remember you need a A1P2 or better - mask

Safety Data:
Link