Hello,

Can anyone recommend any alternatives to 2k paints / primers and fillers for sealing bucks etc.  Is seems 1k systems will be problematic with bonding / mould releasing but 2k looks like evil stuff to work with and prohibitive cost wise for me due to the H&S kit required (3 stage filters for breatheable air supplies, secondary compressor, air fed mask etc..).

Is 1k completely off limit or is it just that it's hit-and-miss to avoid problems?
Replies
brasco
brasco
Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)
Group: Forum Members
Posts: 192, Visits: 305
i know it is totally hillbilly--but you can mix two component primers and use a foam roller to apply..
just sand it smooth after it is cured and you would be fine.
use no reduction (do not thin it) just primer and catalyst. roll on several medium coats and let it almost dry between coats.

and it does work !!


CarbonFiberCreations



neilb
neilb
Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)
Group: Forum Members
Posts: 107, Visits: 504
not as hillbilly as you might think, applying 2k primer with a roller has been around for a long time. it allows jobs to be primered on the shop floor without masking up everything in a big radius. spraying on the shop floor is against H+S regs
fgayford
fgayford
Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)
Group: Forum Members
Posts: 433, Visits: 1.2K
brasco (05/01/2013)
i know it is totally hillbilly--but you can mix two component primers and use a foam roller to apply..
just sand it smooth after it is cured and you would be fine.
use no reduction (do not thin it) just primer and catalyst. roll on several medium coats and let it almost dry between coats.

and it does work !!


Hi Brasco
Us Canadian Hillbilly's have an even cruder way of applying 2 part epoxy primer surfacer. I mix it up like you described and then simply brush it on nice and thick with a cheap chip brush. It works great, sort of like a brushable body filler. Once I have the pits all filled and sanded flat I then spray on a good smooth layer.
Can't argue with results.
Fred
  

brasco
brasco
Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)
Group: Forum Members
Posts: 192, Visits: 305
the original HVLP !!
fgayford (26/01/2013)
brasco (05/01/2013)
i know it is totally hillbilly--but you can mix two component primers and use a foam roller to apply..
just sand it smooth after it is cured and you would be fine.
use no reduction (do not thin it) just primer and catalyst. roll on several medium coats and let it almost dry between coats.

and it does work !!


Hi Brasco
Us Canadian Hillbilly's have an even cruder way of applying 2 part epoxy primer surfacer. I mix it up like you described and then simply brush it on nice and thick with a cheap chip brush. It works great, sort of like a brushable body filler. Once I have the pits all filled and sanded flat I then spray on a good smooth layer.
Can't argue with results.
Fred
  



CarbonFiberCreations



GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Element6 - 12 Years Ago
jamesw - 12 Years Ago
brasco - 12 Years Ago
neilb - 12 Years Ago
fgayford - 12 Years Ago
brasco - 12 Years Ago
Philimon - 12 Years Ago
jamesw - 12 Years Ago
neilb - 12 Years Ago
jamesw - 12 Years Ago
Philimon - 12 Years Ago
             Pictures? :D
matthieutje65 - 12 Years Ago
jamesw - 12 Years Ago
jamesw - 12 Years Ago
matthieutje65 - 12 Years Ago
Philimon - 12 Years Ago
jamesw - 12 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search