Group: Forum Members
Posts: 61,
Visits: 558
|
I'm just about to try a 2k epoxy filler/primer in a can from spraymax (you puncture a bladder with a button on the bottom), this one has no dangerous isocyanates and can be sprayed with a standard carbon type mask for working with epoxy, hopefully that'll polish to a sheen which will be enough to take the mould from, otherwise will then use a gloss coat from them...
Bear in mind not all 2k is the same, certain types are suitable for the right filter masks without needing the pressure fed masks etc (I'm in the same boat)
Will let you know how I get on over the weekend...