Hello there (newbie from France here)

I have a bit of experience with composite as I used to build windsurf and surf boards (amateur style in the 80s 90s), and I'm thinking these days of building another board, and also some furniture things.

And I have a question regarding prepreg, I would be interested in using it (to gain weight the project being quite a "long" board), but my inderstanding is that EPS foam (from which windsurf boards are shaped, not the foam for the sandwich layer) cannot withstand 100°C, or even 80°C, plus it would require quite a big oven.

But how about UV curing prepreg ?

I'm a total newbie in prepreg, but basically my question is whether it is mainstream or not ?
I don't see any products listes on easy composite sites, and could not find a thread discussing it.

So is it still a very specialized technology ? Not really usable by amateurs ? And in general are there some major cons compared to "heat curing prepregs" ? Or is it much more expensive ?
Any info welcome ! Smile
Yves
Edited 3 Years Ago by yvest75
Reply
yvest75
y
Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)
Group: Forum Members
Posts: 2, Visits: 28
Warren (Staff) - 9/27/2022 8:14:53 AM
Its certainly not a common product at the hobby/DIY level for sure. There are a few suppliers who offer it for fairly specific applications. 

Thanks for the answer, and when there are multiple carbon ply, you have to cure it one ply at a time ?