Threads


Author
Message
Dezer
Dezer
Supreme Being (696 reputation)Supreme Being (696 reputation)Supreme Being (696 reputation)Supreme Being (696 reputation)Supreme Being (696 reputation)Supreme Being (696 reputation)Supreme Being (696 reputation)Supreme Being (696 reputation)Supreme Being (696 reputation)
Group: Forum Members
Posts: 74, Visits: 1.8K
Hi, I'm recreating this carbon fiber part, my difficulty is how to add these threads (holes) to my final carbon fiber part.

Any suggestion?

I thought about infusing it with metal on the spot and making the thread with the finished piece, but my fear is that the metal will come out of position.


Reply
Dezer
Dezer
Supreme Being (696 reputation)Supreme Being (696 reputation)Supreme Being (696 reputation)Supreme Being (696 reputation)Supreme Being (696 reputation)Supreme Being (696 reputation)Supreme Being (696 reputation)Supreme Being (696 reputation)Supreme Being (696 reputation)
Group: Forum Members
Posts: 74, Visits: 1.8K
[citar]
[b]Dezer - 28/11/2021 3:19:21 AM[/ b]
Olá, estou recriando esta peça de fibra de carbono. Minha dificuldade é adicionar esses fios (orifícios) à minha peça final de fibra de carbono.

Alguma sugestão?

Pensei em infundi-lo com metal no local e fazer a linha com a peça acabada, mas meu medo é que o metal saia da posição.

[/citar]

Image: 
http://cdn3.volusion.com/rpeq3.x6bgd/v/vspfiles/photos/20005779-3T.jpg?v-cache=1484441372



GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search