90 degree mould and wet layup


Author
Message
The Mould Destroyer
The Mould Destroyer
Supreme Being (295 reputation)Supreme Being (295 reputation)Supreme Being (295 reputation)Supreme Being (295 reputation)Supreme Being (295 reputation)Supreme Being (295 reputation)Supreme Being (295 reputation)Supreme Being (295 reputation)Supreme Being (295 reputation)
Group: Forum Members
Posts: 21, Visits: 332
Hi,
*I've attached the shape of the mould

I have a shape with 90 degrees corners, the part will be then attached snuggly to the side of a flat plywood and glued on 3 sides.I  use peel ply on the inside to get a good bonding surface

The problem is - with a female mould, it does not stick to the contour and I cannot achieve the desired shape
I've considers a male mould that will be much simpler but i would need to first put the peel ply and then the fabric so i dismissed it, although i do prefer it if its possible

Moulds and currently 3d printed for the prototype phase I use Diolen as a cheaper alternative to Kevlar (mostly will be tensile forces on the part)

The outer finish is not that important to me, of course I would prefer it to be nice, cosmetically it's not a must

Any recommendations?


jeffrey bres
j
Supreme Being (659 reputation)Supreme Being (659 reputation)Supreme Being (659 reputation)Supreme Being (659 reputation)Supreme Being (659 reputation)Supreme Being (659 reputation)Supreme Being (659 reputation)Supreme Being (659 reputation)Supreme Being (659 reputation)
Group: Forum Members
Posts: 42, Visits: 469
The Mould Destroyer - 4/24/2021 12:40:02 PM
Hi,
*I've attached the shape of the mould

I have a shape with 90 degrees corners, the part will be then attached snuggly to the side of a flat plywood and glued on 3 sides.I  use peel ply on the inside to get a good bonding surface

The problem is - with a female mould, it does not stick to the contour and I cannot achieve the desired shape
I've considers a male mould that will be much simpler but i would need to first put the peel ply and then the fabric so i dismissed it, although i do prefer it if its possible

Moulds and currently 3d printed for the prototype phase I use Diolen as a cheaper alternative to Kevlar (mostly will be tensile forces on the part)

The outer finish is not that important to me, of course I would prefer it to be nice, cosmetically it's not a must

Any recommendations?


Please note that i am not a profecional!

 If i needed to i would make a fillit in the corner first. Wait till thats sticky and go from there if cosmetics aint importand. 
 Just take a pointy bag fill it with thick paste and put a beat in the corners. Then make a nice concave curve in it with a spatula of some sort and wait. Then go oj with the cloth.


GO