Spread tow


Author
Message
ajb100
ajb100
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 346, Visits: 4.4K
Hope everyone has had a good Xmas!

I've started thinking about the lay up of my next project and decided that spread tow is the way to go for the surface layer.

The problem is I can only seem to find it in 1mtr widths when I really need 1.25 or 1.5. Does anyone know where I can get some that wide? If not ill have to get the EC 1mtr and join it, but want to avoid this at all cost due to the waste and strength etc.

Secondly, has anyone used spread tow before? What's it like to handle? I've been looking at what some of the RC plane guys do and they suggest rolling it out and giving it a light spritz of 3m77, some even put light weight glass just to hold all the fibres together. What I'm making is by no means complex, just a very large multi directional gentle curve so don't think the glass will be needed?

Thanks
Alex
Reply
FLD
FLD
Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)
Group: Forum Members
Posts: 468, Visits: 2.7K
I didn't on mine!  It was outside the moulding area so I just trimmed it off.  With normal carbon I have acetoned it from the opposite side to release the tape but with the spread tow I'd want it there to hold it together.