Hi,

With great difficulty, I got the mould to release from the front bumper. I am happy with the outcome. Just a few questions:

1. Is there an alternative to mould cleaner I can use to clean away the wax?

2. Is there a trick to touching up any imperfections with additional gelcoat?




Edited 5 Years Ago by ats101
Reply
ats101
a
Supreme Being (156 reputation)Supreme Being (156 reputation)Supreme Being (156 reputation)Supreme Being (156 reputation)Supreme Being (156 reputation)Supreme Being (156 reputation)Supreme Being (156 reputation)Supreme Being (156 reputation)Supreme Being (156 reputation)
Group: Forum Members
Posts: 14, Visits: 165
As you mentioned, the problem I have had before is that gelcoat is super hard and takes forever to sand. I have use a fine file to flatten and that works better.