By ats101 - 11/30/2020 9:47:38 AM
Hi,
With great difficulty, I got the mould to release from the front bumper. I am happy with the outcome. Just a few questions:
1. Is there an alternative to mould cleaner I can use to clean away the wax?
2. Is there a trick to touching up any imperfections with additional gelcoat?

|
By ats101 - 12/1/2020 7:39:19 PM
That's some really useful information especially choosing 800 grit as the coarsest of sand paper. That's a mistake I made on project two.
I can imagine the trick with the tape being effective. I will use that and see how I get on.
Thanks, making carbon fibre parts must be your profession?!
|
|