Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Mould Making
»
Mould preparation advice.
Mould preparation advice.
Post Reply
Like
6
Mould preparation advice.
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
ats101
a
ats101
posted 5 Years Ago
ANSWER
HOT
Topic Details
a
Group: Forum Members
Posts: 14,
Visits: 165
Hi,
With great difficulty, I got the mould to release from the front bumper. I am happy with the outcome. Just a few questions:
1. Is there an alternative to mould cleaner I can use to clean away the wax?
2. Is there a trick to touching up any imperfections with additional gelcoat?
Edited
5 Years Ago by
ats101
Reply
Like
6
Reply
ats101
a
ats101
posted 5 Years Ago
ANSWER
HOT
Post Details
a
Group: Forum Members
Posts: 14,
Visits: 165
Thanks Warren.
I have read on this forum that its extremely difficult to get a perfect finish when building up gelcoat and then sanding it flat.
Is this true? The only reason I ask is so I can gauge how much persevere with making it perfect.
Reply
Like
5
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Mould preparation advice.
ats101
-
5 Years Ago
Most of the wax will scrape off plus warm soap and water will help too. There is no special trick to repairs. Sand the effected area then use a small amount of gel to touch up. Solution MW will help...
Warren (Staff)
-
5 Years Ago
Thanks Warren. I have read on this forum that its extremely difficult to get a perfect finish when building up gelcoat and then sanding it flat. Is this true? The only reason I ask is so I can...
ats101
-
5 Years Ago
Nah vinyl gelcoat is pretty forgiving, you CAN get it back to perfect - depends a lot on your skills and technique, as well as the complexity of the area you are repairing. If you build up too much,....
Hanaldo
-
5 Years Ago
As you mentioned, the problem I have had before is that gelcoat is super hard and takes forever to sand. I have use a fine file to flatten and that works better.
ats101
-
5 Years Ago
You shouldn't be using anything as rough as a file, you'll certainly never get that back to a good finish. If I'm compounding anything, whether it is gelcoat or clear coat or resin or whatever - if I...
Hanaldo
-
5 Years Ago
That's some really useful information especially choosing 800 grit as the coarsest of sand paper. That's a mistake I made on project two. I can imagine the trick with the tape being effective. I wil...
ats101
-
5 Years Ago
Post Reply
Like
6
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search