Group: Forum Members
Posts: 10,
Visits: 538
|
Hi, I'm learning infusion and trying to get all the setup with minimal leaks. I'm using EC4 (i've fitted it with ball valve, vacuum gauge and air inlet valve), CP1 catch pot, Greisinger GDH 200-14 gauge at the very end. When pulling vacuum GDH 200-14 starts from 1012 mbar and drops to -2 mbar. Pump side gauge shows -1 bar, catch pot gauge shows -0.95 bar. Questions. 1. I understand that gauges put closer/further from pump will show different values. Should I worry about GDH 200-14 showing -2 or it's just an measurement error I should ignore? 2. After pulling vacuum and clamping hose between pump and catch pot GDH 200-14 shows this: @ 0 min -2 mbar @ 5 min 34 mbar @ 10 min 37 mbar @ 15 min 38 mbar @ 30 min 42 mbar What is acceptable leak rate ?
|